Chitosan was prepared by N-deacetylation of squid pens β-chitin, and N-carboxyethylated chitosan (N-CECS) with different degrees of substitution (DS) were synthesized. DS values of N-CECS derivatives calculated by (1)H nuclear magnetic resonance (NMR) spectroscopy were 0.60, 1.02 and 1.46, respectively. The adsorption capacity of Cu(II) by N-CECS correlated well with the DS and pH ranging from 3.2 to 5.8. The maximum Cu(II) adsorption capacity (qm) of all three N-CECS at pH 5.4 was 207.5mg g(-1), which was 1.4-fold higher than that of chitosan. The adsorption equilibrium process was better described by the Langmuir than Freundlich isotherm model. Adsorption of Cu(II) ion onto N-CECS followed a pseudo-second order mechanism with chemisorption as the rate-limiting step. In a ternary adsorption system, the adsorption capacity of Cu(II) by N-CECS also presented high values, and qm for Cu(II), Cd(II), and Pb(II) were 150.2, 28.8, and 187.9mg g(-1), respectively.
Keywords: Adsorption kinetics; Copper(II) ions; Langmuir isotherm; N-Carboxyethylated chitosan.
Copyright © 2015 Elsevier Ltd. All rights reserved.